Cold-formed vs hot-rolled channels: 14% less steel, 60% more Ix

Two small channels, side by side: a cold-formed 4CS2.5x105 from the AISI tables and a hot-rolled C3X4.1 from the AISC Manual. The cold-formed one is lighter, yet stiffer in both directions. Here is why, and what you give up for it.

Section Designer · 6 min read

4 in 4CS2.5x105, cold-formed 3 in C3X4.1, hot-rolled
Both sections to the same scale. The cold-formed channel is a 0.105 in sheet bent into a 4 × 2.5 in shape with lips. The hot-rolled channel is 3 × 1.41 in, with a 0.17 in web and sloped flanges.

The numbers

Both sections opened from the library in Section Designer, which works out the gross properties from the actual outline:

4CS2.5x105
cold-formed, AISI
C3X4.1
hot-rolled, AISC
Cold-formed
Area, A1.043 in²1.215 in²14% less
Weight3.55 lb/ft4.1 lb/ft13% lighter
Strong axis, Ix2.675 in⁴1.667 in⁴60% more
Weak axis, Iy0.937 in⁴0.199 in⁴4.7 times
Section modulus, Sx1.338 in³1.112 in³20% more
Radius of gyration, ry0.948 in0.405 in2.3 times
Torsion constant, J0.0038 in⁴0.0269 in⁴7 times less

The C3X4.1 values are for Section Designer's model of the rolled shape with its sloped flanges. The AISC Manual lists A = 1.20 in², Ix = 1.65 in⁴ and Iy = 0.191 in⁴, all within 4% of the model, so the comparison holds with either set. The 4CS2.5x105 values match the AISI table, and J for the C3X4.1 is the AISC value.

Why less steel gives more stiffness

The second moment of area adds up every bit of area times the square of its distance from the axis:

I = ∫ y² dA

So a square inch of steel 2 in from the axis adds 4 in⁴, while the same square inch 1 in from the axis adds only 1 in⁴. Where the steel sits matters far more than how much of it there is. Three things put the cold-formed channel's steel farther out:

  1. Thin walls make a bigger shape. A 0.105 in sheet spreads slightly less steel over a 4 × 2.5 in outline, against 3 × 1.41 in for the rolled channel.
  2. The rolled channel keeps steel near the axis. Its web is 0.17 in thick, and the web is the part that does least for Ix and almost nothing for Iy.
  3. The lips put steel at the flange tips, the points farthest from the y axis. That is the main reason Iy is almost five times larger.

Is it a fair comparison?

The sections are not the same depth, and a good part of the Ix gain comes from the extra inch. That is the point, though: with thin sheet, the same weight of steel can be formed into a deeper section. Per pound, the cold-formed channel gives 0.75 in⁴ of Ix for each lb/ft, against 0.41 for the rolled one. The deeper section does need more room, which matters in a wall or floor of fixed depth.

The catch: thin walls

When to use which

Cold-formed sections are light and stiff for repeated, evenly loaded, braced members: wall studs, floor joists, purlins and girts, where the sheathing or deck holds the flanges. Hot-rolled channels are the robust choice for heavier and concentrated loads, for members that are hard to brace, and where the connections are welded or bolted.

Check it yourself

Open Section Designer and insert both sections from the library: the 4CS2.5x105 from the AISI C-sections with lips, and the C3X4.1 from the AISC C channels. The properties panel shows every value in the table above, and you can place the two side by side on the canvas. For a channel of your own dimensions, the free channel calculator shows the working step by step. And for what the elastic and plastic moduli of these sections mean, see elastic vs plastic section modulus.

FAQ

Frequently asked questions

Is a cold-formed channel stronger than a hot-rolled one?

Not necessarily. It can be stiffer for the same weight, because thin walls let the steel form a bigger shape. But thin walls can buckle locally before they yield, so cold-formed strength is checked with effective section properties to AISI S100, not the gross properties.

Why does the cold-formed section have a larger Iy?

The moment of inertia grows with the square of the distance from the axis. The cold-formed channel has wider flanges and lips at the flange tips, the points farthest from the y axis, while the rolled channel keeps much of its steel in a thick web near that axis.

Why is J so small for cold-formed sections?

For open thin-walled sections the torsion constant grows with the cube of the wall thickness, so a 0.105 in wall gives a J about seven times smaller than the thicker rolled channel.

Keep reading

More from the blog

For use by qualified engineers. All results must be checked independently before use in any design. See the Terms of Use.